nitinol
Sign in to saveAlso known as nickel titanium, Nickel Titanium Naval Ordnance Laboratory
metal alloy of nickel and titanium, where the two elements are present in roughly equal atomic percentages
Key facts
- Melting point
- 1,310 °C (2,390 °F)
- Density
- 6.45 g/cm (0.233 lb/cu in)
- Electrical resistivity austenite
- 82 × 10 Ω·cm
- Martensite
- 76 × 10 Ω·cm
- Thermal conductivity austenite
- 0.18 W/cm·K
- Coefficient of thermal expansion austeni
- 11 × 10 /°C
- Magnetic permeability
- < 1.002
- Magnetic susceptibility austenite
- 3.7 × 10 emu/g
- Elastic modulus austenite
- 75–83 GPa (10.9 × 10 ^ –12.0 × 10 ^ psi)
- Yield strength austenite
- 195–690 MPa (28.3–100.1 ksi)